Eggshell Particle Analysis BEI
Biology / Life science, Food / Plant
This is the cross section of an eggshell treated by CP and the number of pores in the eggshell was measured from the SEM image.
| Application | BEI |
|---|---|
| Preprocessing | CP / coating / cross section milling |
| Magnification | x250, x5000 |
| Shooting conditions | Acceleration voltage:5kv、Atomosphere:High vacuum、Detector:BED-C、Working distance:9 mm |
| Related product | JSM-IT700HR InTouchScope™ Scanning Electron Microscope JSM-IT710HR Scanning Electron Microscope IB-19520CCP CROSS SECTION POLISHER™ |