Eggshell BEI

Biology / Life science, Food / Plant

This is the cross section of an eggshell treated by CP and the number of pores in the eggshell was measured from the SEM image.

Application BEI
Preprocessing CP / coating / cross section milling
Magnification x250, x5000
Shooting conditions Acceleration voltage:5kv、Atomosphere:High vacuum、Detector:BED-C、Working distance:9 mm
Related product JSM-IT700HR InTouchScope™ Scanning Electron Microscope
JSM-IT710HR Scanning Electron Microscope
IB-19520CCP CROSS SECTION POLISHER™

Related data

Particle Analysis BEI

Close
Notice

Are you a medical professional or personnel engaged in medical care?

Yes

No

Please be reminded that these pages are not intended to provide the general public with information about the products.

JEOL Instrument Basics

Easy explanation about mechanisms and
applications of JEOL products

Contacts

JEOL provides a variety of support services to ensure that our customers can use our products with peace of mind.
Please feel free to contact us.