All-solid-state battery silicon negative electrode material Distribution of Li  BEI

Battery, Automobile

All-solid-state batteries are batteries in which the electrolyte is replaced by a solid, and are attracting attention as a next-generation battery because they are safer than liquid electrolytes and can have a larger capacity. When charging, the battery is charged by the Li contained in the solid electrolyte moving to the silicon anode material.

Contrast differences between particles suggest differences in composition, density, and crystal (orientation).

①Si anode (mixture of Si particles, conductive assistant, and solid electrolyte)
②Sulfide based solid electrolyte
③Si particle

Application BEI
Preprocessing CP
Shooting conditions Acceleration voltage:3 kV,High vacuum mode
Related information Solid-State Battery Note
Related product JSM-IT800 Schottky Field Emission Scanning Electron Microscope
Close
Notice

Are you a medical professional or personnel engaged in medical care?

Yes

No

Please be reminded that these pages are not intended to provide the general public with information about the products.

Science Basics

Easy explanation about mechanisms and
applications of JEOL products

Contacts

JEOL provides a variety of support services to ensure that our customers can use our products with peace of mind.
Please feel free to contact us.