Glass epoxy resin SEI

Plastics / Polymer

A secondary electron image of an Au-coated glass epoxy resin fracture surface. Compared with the backscattered electron image, the secondary electron image allows the observaiton of brittle fracture of the resin.

Application SEI
Magnification ×1,500
Shooting conditions 15 kV,HV

Related data

Resin SEI

Glass epoxy resin BEI