Our paper has been published in "Crystal Growth & Design"
Release Date: 2025/10/29
Our paper has been published in "Crystal Growth & Design" based on collaboration between Yonsei University, Institute of Basic Science, Kyoto University and JEOL Ltd. The paper reported the significantly enhanced proton mobility by adjusting cation component in isostructural HOFs (hydrogen-bonded organic frameworks). We have revealed the conductivity of protons by PFG (pulsed field gradient) NMR method. The paper was selected for supplemental journal cover. The project was led by Yonsei University.
Enhancement of Mobile Protons Induced by Ammonia in Isostructural Hydrogen-Bonded Organic Frameworks, Cryst. Growth Des. 25(2025) 8332-8338.