Adapting a JEM-2100F for Magnetic Imaging by Lorentz TEM

JEOLnews Volume 47, Number 1, 2012 Amit Kohn and Avihay Habibi
Department of Materials Engineering and the Ilse Katz
Institute for Nanoscale Science and Technology, Ben-Gurion
University of the Negev

Lorentz TEM enables to map quantitatively magnetic induction fields in the sample. A specifically designed objective lens, a coherent electron source, and a biprism filament can achieve magnetic imaging at the nanometer scale through off-axis electron holography experiments. However, this equipment is specialized and therefore not suited to many microscopy labs. In this article, we describe an adaptation of a conventional JEM-2100F for Lorentz phase microscopy, namely Fresnel-contrast imaging. Since a biprism filament is installed on this microscope, we evaluate the capabilities of the Fresnel-contrast magnetic imaging. We show that a relatively simple and low-cost adaptation enables quantitative magnetic and electrostatic mapping on a conventional TEM.

Please see the PDF file for the additional information.

PDF 5.87MB
Close
Notice

Are you a medical professional or personnel engaged in medical care?

Yes

No

Please be reminded that these pages are not intended to provide the general public with information about the products.

JEOL Instrument Basics

Easy explanation about mechanisms and
applications of JEOL products

Contacts

JEOL provides a variety of support services to ensure that our customers can use our products with peace of mind.
Please feel free to contact us.