analytical electron microscopy, AEM
analytical electron microscopy
A microscopy method that adds analytical functions, such as EDS and EELS to a TEM, in order to perform qualitative and quantitative analysis of elements and/or electronic structure analysis from micro- or nano-areas subjected to TEM observation.