diffuse streak
diffuse streak
"Diffuse streak" means the streak intensity appearing in a (selected-area) diffraction pattern. The streak is produced from planar lattice defects (stacking faults, etc.) or linear lattice defects (atomic columns of different species or vacancy columns). Disorder of crystal structures can be deduced from the analysis of the diffuse streak.