epitaxy
epitaxy
"Epitaxy" is a technique to deposit and grow a crystalline film on a crystalline substrate using vacuum evaporation (deposition) or chemical vapor deposition (CVD), etc. In epitaxy, the crystalline film formed has a specific orientation relation with the substrate crystal.