Ultrafast MAS of heavy 1/2-spin nuclei:Ultra-wideline 119Sn solid-state NMR at 75 kHz MAS

NM160006E

Ultrawide-line 119Sn solid-state NMR spectra of tin(II) oxide (SnO) were collected at low and ultrafast Magic Angle Spinning (MAS) (Fig. 1) [1].
The ultrafast MAS approach offers following benefits over the low MAS approach: simple setup, straightforward data acquisition and processing, efficient excitation, reduced number of spinning sidebands (SSB) resulting in significant spectral simplification, and increased mass sensitivity allowing the fast study of small amounts of material. In addition, the ultrafast MAS experiments provide optimal conditions for the extraction of the chemical shift anisotropy tensor parameters, anisotropy, and asymmetry for heavy 1/2-spin nuclei [1].

Fig.1 Comparison of experimental (blue) and simulated (red) 119Sn NMR spectra of SnO. a) Nine subspectra were collected and added to give a full spectrum in the case of slow MAS (11.8 kHz, 4mm o.d. rotor). b) At ultrafast MAS (43–75 kHz, 1mm o.d. rotor), a single-pulse experiment was sufficient to excite and record the full pattern.

Reference

[1] A.-C. Pöppler, J.-P. Demers, M. Malon, A.P. Singh, H.W. Roesky, Y. Nishiyama, A. Lange, ChemPhysChem 17 (2016) 812-816.

SEARCH APPLICATIONS

Solutions by field

Close
Notice

Are you a medical professional or personnel engaged in medical care?

Yes

No

Please be reminded that these pages are not intended to provide the general public with information about the products.

JEOL Instrument Basics

Easy explanation about mechanisms and
applications of JEOL products

Contacts

JEOL provides a variety of support services to ensure that our customers can use our products with peace of mind.
Please feel free to contact us.