FGMAS probe

NM080006E

Realization of high resolution measurement of semi-solid sample by high speed MAS. 
Easy inverse measurement by magnetic field gradient function further.

Feature

"FG(Field Gradient)MAS(Magic Angle Spinning) Probe" is a probe with magnetic field gradient which enables high speed MAS. The target samples are so-called semi-solid sample such as cream, gel, paste samples, or very viscous sample such as ionic liquid, as well as tissue from a living body and sample combined with resin for solid-phase synthesis. Further, high resolution measurement of rubber samples which used to be analyzed by liquid (latex state) NMR or solid NMR, is possible with high speed MAS by using this method.

Specification

Observation nuclei:1H, 13
Applicable Magnetic Field:400 to 600MHz
Temperature Variable Range:Room Temperature to 50°C
2H NMR Lock, magnetic field gradient function provided.

4 mm type
 Spinning speed:17 kHz
 Sample volume:37 μL

3.2mm type
 Spinning speed:22 kHz
 Sample volume:27 μL
FGMAS probe

Soymilk mayonnaise


Ingredients
Canola oil, Soymilk, Cider Vinegar, Salt, Sugars

MAS speed:5 kHz

Vulcanized Natural Rubber


Croosslink density:1.36×10-4 moI/cm3

Sample kindly provided by Dr. Seiichi Kawahara
(Nagaoka University of Technology).

MAS speed:17 kHz

In most cases of rubber sample, the structure of main chain is already known, and the analysis of side chain is the main.
However, signal coming from side chain is very small, so stable measurement becomes important.
In addition, inverse two-dimensional measurement of 1H observation, the cross peak coming from the side chain is buried in the cross peak coming from the main chain, so, some kind of works to select out or to delete signal coming from the main chain, are necessary.


Measurement Time:
About 35h 45min.

SEARCH APPLICATIONS

Solutions by field

Close
Notice

Are you a medical professional or personnel engaged in medical care?

Yes

No

Please be reminded that these pages are not intended to provide the general public with information about the products.

JEOL Instrument Basics

Easy explanation about mechanisms and
applications of JEOL products

Contacts

JEOL provides a variety of support services to ensure that our customers can use our products with peace of mind.
Please feel free to contact us.