PFG-COSY Spectrum(1scan)
PFG-COSY Spectrum(1scan)
PFG-HSQC Spectrum(4scan)
PFG-HSQC Spectrum(4scan)
PFG-HMBC Spectrum(4scan)
PFG-HMBC Spectrum(4scan)
Sample:Commercial Polycaprolactone diol (Average Molecular Weight: 830)
Solvent:CDCl3
Spectrometer:JNM-ECX400
Probe:T10A AT/FG

A JEOL high-resolution 10mm probe is equipped with a field gradient coil. By using  field gradient pulses, various measurements can be performed in a short time, and  good spectra without t1 noise can easily be obtained in inverse measurements.
In the case that a large amount of samples are available like polymer samples,  sensitivity enhancement using a 10mm sample tube is effective. High sensitivity of  a new 10mm probe with a field gradient coil is useful in multi-dimensional NMR  measurements.

SEARCH APPLICATIONS

Close
Notice

Are you a medical professional or personnel engaged in medical care?

Yes

No

Please be reminded that these pages are not intended to provide the general public with information about the products.

JEOL Instrument Basics

Easy explanation about mechanisms and
applications of JEOL products

Contacts

JEOL provides a variety of support services to ensure that our customers can use our products with peace of mind.
Please feel free to contact us.