10mm special probe for silicon (29Si) measurements

NM060004E

In 29Si NMR measurements, background signals are usually of a problem; even though background from sample tubes is reduced by using PTFE tubes, background from silicon parts of the probe, if any, cannot be removed.
In this special probe, all the silicon materials are replaced by carbon materials. As shown below, background signals arising from silicon materials of the standard probe are removed when the special probe is used. This probe is highly recommended for the users suffering from silicon background.

29Si spectra without samples

Standard probe


Special probe

Specifications
Sample tube o.d.

10mm

Observation nucleus

29Si

Irradiation nucleus 1H
NMR lock nucleus 2H
90°pulse (29Si) 29Si < 25μs
Temp. range RT to +80℃

* This probe is specially designed for 29Si, and so background may appear for the other nuclei.

29Si専用ブローブ
External view

SEARCH APPLICATIONS

Close
Notice

Are you a medical professional or personnel engaged in medical care?

Yes

No

Please be reminded that these pages are not intended to provide the general public with information about the products.

JEOL Instrument Basics

Easy explanation about mechanisms and
applications of JEOL products

Contacts

JEOL provides a variety of support services to ensure that our customers can use our products with peace of mind.
Please feel free to contact us.