Close Btn

Select Your Regional site

Close

High-resolution 10mm probe

NM050009E


Fig.1 13C{1H} spectrum using a high-resolution 10mm probe
Sample: commercial polypropylene/ODCB (o-dichloro benzene-d4)
Spectrometer: JNM-ECA600,  Accumulation: 20,000scan, Temperature: 130℃


Fig.2 13C{1H} spectrum using a 5mm probe
Sample: commercial polypropylene/ODCB
Spectrometer: 750MHz,  Accumulation: 20,000scan, Temperature: 110℃
* Data are by courtesy of Prof. K. Ute of Osaka University.

A high-resolution 10mm probe achieves high sensitivity from a large  volume of samples as well as high resolution due to advanced probe  technology enhancing homogeneity of the magnetic field for that  volume.
A 13C spectrum observed using a 10mm probe (Fig. 1) exhibits resolution as high as that obtained using a 5mm probe (Fig. 2), with  much higher sensitivity. Owing to sufficient resolution and sensitivity, it is possible to quantify atactic parts of polypropylene contained  by about 0.1%.
Thus, a high-resolution 10mm probe is useful in the research of  polymers.

SEARCH APPLICATIONS

Close
Notice

Are you a medical professional or personnel engaged in medical care?

Yes

No

Please be reminded that these pages are not intended to provide the general public with information about the products.

JEOL Instrument Basics

Easy explanation about mechanisms and
applications of JEOL products

Contacts

JEOL provides a variety of support services to ensure that our customers can use our products with peace of mind.
Please feel free to contact us.