Strong interaction between light and electrons (3) "Strong coupling state of ferromagnetic thin film"

ER200008E

Coupling constant (𝑔𝑚) between microwave photon and electron spins is proportional to the square root of spin numbers as shown in eq.(1) of "Application Note ER200007E ". Therefore, FMR measurements using ferromagnets which include many spins and especially have narrow line widths do not work well, because spins in ferromagnets interact strongly with microwave photon, and achieve to "strong coupling" state larger than the state of "Purcell effect". Figure 1(a) is an example that shows the obtained unexpected spectrum in the strong coupling state. Normal FMR spectrum can be obtained as shown in Fig.1(d), if the filling factor is reduced and the system moves to a "weak coupling" state.

Fig.1 FMR spectral examples using ferromagnetic thin film (yttrium iron garnet(YIG)).

Fig.1 FMR spectral examples using ferromagnetic thin film (yttrium iron garnet(YIG)).

(a) Extraordinary spectrum obtained in the strong coupling state. (b) Sample position in the cavity. This produces a spectrum of (a). (c) Ordinary spectrum obtained in the weak coupling state. (d) Sample position in the cavity. This produces a spectrum of (c). (e) YIG thin film sample.

Frequency spectra of the cavity in "strong coupling" state.

図2 An example of frequency spectra of YIG-CMP system.

図2 An example of frequency spectra of YIG-CMP system.

Figure 2 is a mapping chart that frequency spectra (Q-dip) of the cavity are arrayed on the respective measured magnetic fields. Different from the "Purcell effect", as closing to the resonant field, spectral peak splits to two and shifts repulsively. The coupling constant can be estimated as 𝑔𝑚 ∕ 2𝜋 = 36 MHz from the splitting width of spectrum on the resonant magnetic field which an arrow indicates. This system is regarded as strong coupling state, because 𝑔𝑚 is larger than kc 𝑎𝑛𝑑 𝛾𝑚 , where QL is ca 8200 (kc ∕ 2𝜋 = 0.55 MHz), and the spectral half width is ca 75 μT (𝛾𝑚 / 2𝜋=2.1 MHz). The system that a cavity and a magnon belong to strong coupling state is called "cavity magnon polariton (CMP)". The CMP system is recently gathering a lot attention in quantum optics and quantum information, as an artificial quantum or quasi particle which is unified between microwave photon and spins of a magnon[1].

Reference: [1] M. Harder and C.-M. Hu, Solid State Physics 69, 47 (2018).

Please see the PDF file for the additional information.
Another window opens when you click.

PDF 304.3KB

SEARCH APPLICATIONS

Close
Notice

Are you a medical professional or personnel engaged in medical care?

Yes

No

Please be reminded that these pages are not intended to provide the general public with information about the products.

JEOL Instrument Basics

Easy explanation about mechanisms and
applications of JEOL products

Contacts

JEOL provides a variety of support services to ensure that our customers can use our products with peace of mind.
Please feel free to contact us.