Line shape of an electromotive force (emf) spectrum using the spin pumping effect by ferromagnetic resonance (FMR) is regarded as the convoluted spectrum consisted the two emf components, i.e. the inverse spin-Hall emf (VISHE) and the amomalous Hall emf (VAHE). It is known that this is expressed in eq. (1)[1]

Especially, the anomalous Hall effect makes the shape change according to the way of affection of the electric component of microwaves and the properties of samples. Therefore, it is necessary to analyze the obtained spectrum and to distinguish the mixed components by eq.(1). It makes possible to elucidate the effect of the pure spin current.

Sample and method

The dependences of microwave power on FMR spectrum and the emf amplitude (Vemf) were measured simultaneously using the same sample reported on JEOL application note [ER190002E] .

The power dependence of microwave on FMR and the ISHE (VISHE) 

Vobs. (Fig. 1) shows is an obtained Vemf spectrum by an experiment. VISHE and VAHE were divided by fitting using eq. (1) after conversion of obtained differential spectrum (Vobs.) to an integrated one because conventional FMR method adopted a magnetic field modulation scheme.
As shown in Fig. 2, FMR spectra (Fig. 2 (a)) are proportional to the square root of the irradiated microwave power. On the other hand, VISHE spectra (Fig. 2 (b)) are proportional to the irradiated microwave power[2].


図1 逆スピンホール効果の線型解析例
Fig. 1 Spectral deconvolution of Vemf spectrum.
Fig. 2 The irradiated power dependence of FMR spectra and VISHE spectra.

References

[1] E. Saitoh, M. Ueda, H. Miyajima and G. Tatara, Appl. Phys. Let. 88(2006), 182509.
[2] K. Ando, S. Takahashi, J. Ieda, Y. Kajiwara, H. Nakayama, T. Yoshino, K. Harii, Y. Fujikawa, M. Matsuo, S. Maekawa, and E. Saitoh, J. Appl. Phys. 109(2011), 103913.

If you want to see a printed version, please click this PDF file.

PDF 312KB

SEARCH APPLICATIONS

Close
Notice

Are you a medical professional or personnel engaged in medical care?

Yes

No

Please be reminded that these pages are not intended to provide the general public with information about the products.

JEOL Instrument Basics

Easy explanation about mechanisms and
applications of JEOL products

Contacts

JEOL provides a variety of support services to ensure that our customers can use our products with peace of mind.
Please feel free to contact us.