Close Btn

Select Your Regional site

Close

Ferromagnetic thin film and spin current (2) - Inverse spin-Hall effect

ER190003E

The ferromagnetic resonance (FMR) spectrum of a bilayer thin film consisting of ferromagnetic and non magnetic metal shows different line widths compared to a monolayer film. This is understood as an effect of flowing out of pure spin current to non magnetic metal on the interface of the bilayer which is due to the spin pumping effect which transfers spin angular momentum of the ferromagnet by FMR[1]. So, how can we detect this pure spin current? One of the well known methods is to use ESR instrument[2]. As shown in Fig.1, when the spin current (JS) flows vertically down in the thin film located in an applied static magnetic field (B0), the electric current (JC) generates toward the orthogonal direction to both the magnetization (σ // B0) and JS. It is called inverse spin-Hall effect (ISHE). Pure spin current can be measured indirectly by detecting electromotive force (Vemf) of thin film[2].

図1.逆スピンホール効果の模式図
Fig. 1 Drawing of inverse spin-Hall effect

Sample and method

The electromotive force (Vemf) of Pd and the Py-FMR spectrum were measured simultaneously using the same sample shown in JEOL application note [ER190002E].

FMR and inverse spin-Hall effect (VISHE)

As shown in Fig. 2, an electromotive force (Vemf) spectrum was obtained at the same magnetic field of FMR spectrum. Analysis of line shape, angular dependence and irradiated microwave power dependence enable us to extract information of inverse spin-Hall electromotive force (VISHE)and understand many properties of spin current that flows in thin film devices.

図2 Py/Pd金属2層薄膜のFMRスペクトルとVemfスペクトル


Fig. 2 Py-FMR spectrum and Vemf spectrum of Py/Pd bilayer

 Set Parameters & Conditions

Sample Py(Ni78Fe22)/Pd
Angle [deg.] Bo // Film plane
Temperature [°C] 27
NW Frequency [MHz] 9435.45
MW Power [mW] 64
Bo [mT] 115 - 265
Mod. Width [mT] 1
Mod. Freq. [kHz] 100
Mod. Phase [deg.] -60
Sweep Time [s] 30
Accumulation 64
Amp. Gain 10 (CH1:FMR)
105 (CH2[CN107]:VISHE)
Tc [s] 0.01

References

[1] Y. Tserkovnyak, A. Brataas, and G. E. W. Bauer, Phys. Rev. Lett. 88(2002), 117601.
[2] E. Saitoh, M. Ueda, H. Miyajima and G. Tatara, Appl. Phys. Let. 88(2006), 182509.

Please see the PDF file for the additional information.
Another window opens when you click.

PDF 332KB

SEARCH APPLICATIONS

Close
Notice

Are you a medical professional or personnel engaged in medical care?

Yes

No

Please be reminded that these pages are not intended to provide the general public with information about the products.

JEOL Instrument Basics

Easy explanation about mechanisms and
applications of JEOL products

Contacts

JEOL provides a variety of support services to ensure that our customers can use our products with peace of mind.
Please feel free to contact us.