Degradation Study of Heat-Resistant PAI - Ⅱ -

ER170004

In the Application Note ER-150004, an evaluation of the thermal degradation of heat-resistant polyamide-imide (PAI) resin was described. The response to transient thermal loads was investigated by increasing the temperature of the resin in steps and taking measurements. This time, we introduce a study of the changes in the radical species during the thermal degradation process, using PAI with a different thermal response in the low temperature range.

The assessment was performed as follows:

  • Specimen: Commercial PAI (Heat resistance 250°C), 10 mm length of a cylindrical rod of diameter 3 mm
  • Instrument: JES-X320 + 400°C-VT (variable temperature device)
  • Measurement: After measuring the sample at room temperature, heating at 200 or 350°C was performed for 80 minutes and measurements were made. Then, the room temperature measurement was repeated.

The results are shown in Figures 1 and 2. As previously reported, PAI contains 2 species of radicals even at room temperature (-CO· and nitrogen-derived radicals). The -CO· radical increases when the material is heated.
The Mn marker seen in both figures was the same amount, but the intensity of the signal is smaller in Figure 2. This means that a larger amount of radicals were generated at 350°C. After heating to 200°C, the radical content returned to nearly the initial levels after cooling. After heating to 350°C, however, the radical content remained significantly higher than the initial levels, even after cooling. This reveals that heating PAI to 350°C causes new, relatively stable radicals to be generated.
The g-value for the main radicals was 2.004 (C-O·) both before heating and for the heating to 200°C. This changed to g = 2.003 (C·) as a result of heating to 350℃. The observed changes in the g-value indicate that the resin has been denatured.

Fig. 1 Heating-induced changes in radicals in PAI(200℃)

Fig. 1 Heating-induced changes in radicals in PAI (200°C)

Fig. 2 Heating-induced changes in radicals in PAI(350℃)

Fig. 2 Heating-induced changes in radicals in PAI (350°C)

As this shows, using ESR to assess the thermal degradation of resin from the perspective of radical generation can be expected to provide new information about the degradation mechanisms. The 400°C-VT can be effectively utilized to assess thermal degradation.

Please see the PDF file for the additional information.
Another window opens when you click.

PDF 474.2KB

SEARCH APPLICATIONS

Solutions by field

Close
Notice

Are you a medical professional or personnel engaged in medical care?

Yes

No

Please be reminded that these pages are not intended to provide the general public with information about the products.

JEOL Instrument Basics

Easy explanation about mechanisms and
applications of JEOL products

Contacts

JEOL provides a variety of support services to ensure that our customers can use our products with peace of mind.
Please feel free to contact us.