Analysis of high molecular weight polystyrene standards by using JMS-S3000 "SpiralTOF™" with Linear TOF option.

MSTips No.199

An example of the analysis of low molecular weight Polystyrene (PS) by using JMS-S3000 SpiralTOF™ MALDI-TOFMS was already shown in MSTips No.163 .
This time, high molecular weight polystyrene standards (TSKgel Standard Polystyrene F-4 (Mw = 3.72x104), F-10 (Mw = 9.89x104), and F-20 (Mw = 1.89x105), Tosoh Corporation) were analyzed by using JMS-S3000 SpiralTOF™ with Linear TOF option(Fig. 1).
For F-4, peaks were observed at every 104 u, which is the repeating unit of PS. For both F-10 and F-20, expected distributions around their respective average molecular weights were obtained (Fig. 2).
Wide applications of the Linear TOF option for the analyses of high molecular weight synthetic polymers are expected.
Fig.1 Repeating unit

Fig.1 Repeating unit
(C8H8=104.0626)

Fig.2 Mass spectra of PS using LinearTOF option.

Please see the PDF file for the additional information.
Another window opens when you click.

PDF 594KB

Related Products

Solutions by field

Close
Notice

Are you a medical professional or personnel engaged in medical care?

Yes

No

Please be reminded that these pages are not intended to provide the general public with information about the products.

JEOL Instrument Basics

Easy explanation about mechanisms and
applications of JEOL products

Contacts

JEOL provides a variety of support services to ensure that our customers can use our products with peace of mind.
Please feel free to contact us.