Preparation of a High Quality Cross Section of a Bone Tissue for SEM
-Application of the Cross-section Polisher to a Biological Specimen-
A bone tissue of a mouse tail, composed of hard and soft materials, was polished with the Cross-section Polisher (CP) for obtaining wide and smooth cross-section.The prepared specimen was observed with a SEM and analyzed with an EDS.
-