Application of Scanning Electron Microscope to Dislocation Imaging in Steel

JEOLnews Volume 46, Number 1,2011 Masaaki Sugiyama窶 and Masateru Shibata窶窶

窶 Advanced Technology Research Laboratories,Nippon Steel Corporation
窶窶 SM Business Unit, JEOL Ltd.

Dislocation imaging using the scanning electron microscope with super hybrid lens will be demonstrated to investigate the dislocation cell walls and single dislocations inside cells introduced by shear deformation in conventional steel. The resolution of the dislocation by electron channeling contrast imaging method is similar to that obtained by conventional TEM observation, and a new approach for the study of dislocations which is possible to detect the heterogeneity of the deformation microstructure will be expected on the view point of the advantage of SEM-BSE techniques. There are two different imaging configurations for doing ECCI, one is a fore-scatter geometry, and the other is a back-scatter one. In the present study, the latter case is utilized, which has advantages for little restriction to the sample size and shape and several applications to the stage design in SEM. Since there are some discussions in the contrast mechanism, the improvement of the backscattering electron detector will bring us several ideas for the application of microscopy to the dislocation study with a combination of the conventional TEM technique.

Please see the PDF file for the additional information.

PDF 5.49MB

Solutions by field

Close
Notice

Are you a medical professional or personnel engaged in medical care?

Yes

No

Please be reminded that these pages are not intended to provide the general public with information about the products.

JEOL Instrument Basics

Easy explanation about mechanisms and
applications of JEOL products

Contacts

JEOL provides a variety of support services to ensure that our customers can use our products with peace of mind.
Please feel free to contact us.