Measurement of Synthetic Polymers [3]: Polyethylene Glycol

MSTips No.165

Polyethylene glycol (PEG) 1000 and 8000 were measured by using the JMS-S3000 SpiralTOF. The [M+H]+ peaks for PEG with the basic monomer units of 44u (Fig. 1) were observed for each sample. The mass spectrum for PEG1000 and an expanded view around m/z 1,000 are shown in Fig. 2. The resolving power at m/z 1009 is approximately 60,000 (FWHM). The mass difference between the 21, 22 and 23-mers showed very good agreement with the theoretical mass of the PEG monomer.The full mass spectrum for PEG8000 is shown in Fig. 3(a). The comparison between the observed and simulated isotopic pattern (R 35,000) for the 226mer are shown in Fig. 3(b). The observed isotopic pattern is in very good agreement with the calculated isotopic distribution.

Please see the PDF file for the additional information.
Another window opens when you click.

PDF313KB

Related Products

Solutions by field

Close
Notice

Are you a medical professional or personnel engaged in medical care?

Yes

No

Please be reminded that these pages are not intended to provide the general public with information about the products.

JEOL Instrument Basics

Easy explanation about mechanisms and
applications of JEOL products

Contacts

JEOL provides a variety of support services to ensure that our customers can use our products with peace of mind.
Please feel free to contact us.