Close Btn

Select Your Regional site

Close

Measurement of Synthetic Polymers [2]: Polymethal Methacrylate

MSTips No.164

Polymethyl methacrylate (PMMA) 4000 was measured by using the JMS-S3000 SpiralTOF. The [M+H]+ peaks for PMMA with the basic monomer units of 100u (Fig.1) were observed for this sample. The full PMMA mass spectrum and an expanded view around m/z 4000 are shown in Fig. 2(a) and (b), respectively. The resolving power at m/z 4,000 was approximately 45,000 (FWHM). Also, the mass differences between the 39, 40, and 41-mers had a very good match with the theoretical mass number (100.0524) of the PMMA repeat unit (C5H8O2). A comparison between the 40-mer’s observed and simulated isotopic patterns is shown in Fig. 2(c). The observed isotopic pattern is in very good agreement with the calculated isotopic distribution.

Please see the PDF file for the additional information.
Another window opens when you click.

PDF 281KB

Related Products

Solutions by field

Close
Notice

Are you a medical professional or personnel engaged in medical care?

Yes

No

Please be reminded that these pages are not intended to provide the general public with information about the products.

JEOL Instrument Basics

Easy explanation about mechanisms and
applications of JEOL products

Contacts

JEOL provides a variety of support services to ensure that our customers can use our products with peace of mind.
Please feel free to contact us.