GC/TOFMS analysis of high boiling point compounds:cholesterol and Irganox® 1010

MS Tips No.123

As examples of GC/MS analyses of high boiling point compounds, cholesterol and Irganox® 1010, an anti-oxidant additive for polymers, were analyzed. The analyses were performed with electron ionization (EI) and field ionization (FI,) which is a soft ionization method.
Please see the PDF file for the additional information.
Another window opens when you click.

PDF 130KB