A paper by a collaboration with Okinawa Institute of Science and Technology Graduate University et al. and JEOL RESONANCE Inc. has been published in "Chemical Communications"
Release Date: 2019/12/11
A paper by a collaboration with Okinawa Institute of Science and Technology Graduate University et al. and JEOL RESONANCE Inc. has been published in "Chemical Communications".
“Highly sensitive mechano-controlled luminescence in polymer
films modified by dynamic CuI-based cross-linkers”
Digital version is available online.
https://pubs.rsc.org/en/content/articlelanding/2019/CC/C9CC08354E#!divAbstract