Beyond Morphology and Composition:
An Integrated SEM-EDS-Raman Approach for Advanced Materials Characterization

Release Date: 2026/08/25

Correlative SEM-EDS-Raman analysis provides a powerful approach for understanding materials from multiple perspectives. By combining morphological, elemental, and molecular information within a single workflow, researchers can gain deeper insights into material properties and behavior. This webinar introduces the principles, advantages, and application examples of integrated SEM-EDS-Raman characterization across a variety of advanced materials.

This seminar will be delivered online in an on-demand format, available for a limited time. Enjoy the flexibility to view the content anytime, anywhere during the designated period.

By attending this webinar you will learn…

  • A method that combines SEM, EDS, and Raman data for a more complete view of materials.

  • How to identify molecular and chemical-state information beyond SEM-EDS.

  • How to explore practical applications across a wide range of advanced materials.

Who should attend?

  • Researchers seeking deeper materials characterization beyond SEM-EDS.

  • Scientists interested in chemical-state and molecular analysis methods.

  • SEM or EDS users considering Raman spectroscopy for their workflow.

Related Products

JSM-IT810 Schottky Field Emission Scanning Electron Microscope

Presenter

Jinfeng Lu

EP Application Department
EP Business Unit
SI Business Operations
JEOL Ltd.

On-Demand Viewing Period

Sep 23 (Wed) to Sep 25 (Fri), 2026

  • Please note that the dates are based on Japan Standard Time (JST). Kindly check your local time zone when accessing the content.

Fee

Free

Presentation Materials

You can download these materials after completing the post-presentation survey.

Recording

The recording of the webinar will be posted on the "Webinar Archive" page at a later date.
We will notify you via our e-newsletter and social media once it becomes available.

Q&A Session

There will be no Q&A session following the presentation.

Contacts

E-mail:sales1[at]jeol.co.jp
Demand Generation Div.
JEOL Ltd.

  • please use @ for [at]

Registration

Please register here.

  • For those who have registered, we will send you information on how to access the video viewing page approximately three days before the scheduled start date. We kindly ask for your patience until then.

  • Please note that we may not be able to accept registrations from other companies in the same industry.

Close
Notice

Are you a medical professional or personnel engaged in medical care?

Yes

No

Please be reminded that these pages are not intended to provide the general public with information about the products.