This plasma source can be incorporated into a vacuum chamber and generate high-density plasma. The plasma source can be used as Ion Plating (Plasma Assisted Deposition) for thin films, especially optical thin films. Film quality such as density, adhesion, flatness, index of refraction and absorption are improved by comparison with usual vacuum deposition method.

BS-80011BPG
BS-80011BPG

Example of Installation:

Features:

  • Generate high density plasma in a vacuum chamber
  • Available for large area
  • High deposition late (same level as vacuum evaporation)
  • Reactive deposition are possible
  • Low absorption (oxidation action)
  • Production of environmentally stable films
  • Index of refraction are improved
  • Adhesion, film density and film flatness are improved
  • Can select from irradiation-beam and reflection-beam methods

Example of Optical Thin Film:
(click to enlarge)

Specification:

  • Plasma output: Up to 6.08kW
    (Discharge voltage: 160V, Discharge current: 38A)
  • Operating pressure: 1×10-2 to 1×10-1 Pa
    (Ar, O2 or N2 environment)
  • Discharge gas: 8 to 20 mL/min (Ar gas)
  • Cooling water: 7 to 10 L/min (10 to 25°C)

Technical Information:

[ download technical information ]

  

Please Note

Not all JEOL products are available in every country. For specific information and more details about JEOL products available in your area, contact your local JEOL office or sales representative. Thank you.

  

 
  Copyright 2006-2012 JEOL Ltd. | Privacy Statement | Terms Of Use
  Designed & Powered by the Swanzey Internet Group